Sign In | Join Free | My benadorassociates.com |
|
Brand Name : xinzheng
Model Number : 1j50
Certification : ISO, EN, MTC
Place of Origin : CHINA
MOQ : 1 MT
Price : 1000-3000 Usd / Mt
Payment Terms : L/C, D/P, T/T, Western Union, MoneyGram
Supply Ability : 4000 MT PER week
Delivery Time : 5-25 Days
Packaging Details : Standard seaworthy export package
Standard : 1j50
Grade : Ni50, E11a, 50H, Hy-Ra49, PB
Certificate : Mill MTC ,Third party Inspection
Process : Cold rolled
Thickness : 0.15mm- 120mm
Width : 10mm-2030mm
Length : Max 18000mm
Surface finish : Brushed ,Mirror , 2B
Ualloy-1J50 is a nickel–iron magnetic alloy, with about 50% nickel and 48% iron content. It is derived in accordance with permalloy. It has characteristics of high permeability and high saturation magnetic flux density.
Alloy melting in a vacuum medium, cast into ingots, after hot forging blanks made of sheet metal, and then after hot rolling, pickling, surface treatment, cold rolling into finished products.
Ualloy-1J50 iron-nickel alloy( soft magnetic alloy) mostly in an alternating magnetic field used mainly for high magnetic yoke, sensitive relays, low-loss micro-motor, small power transformers, pulse transformer, transistor switches, magnetic amplifier magnetic modulator, sensitive signal input and output transformers, magnetic heading aviation instrumentation magnetic sensor, magnetic susceptibility measurement instrument components, precision meter movable piece and the stator magnetic shielding and magnetic temperature compensation element.
Produc Forms : Sheet, plate , Coil , Strip .wire , Pipe, Tube ,Bar , Profile, Round, Flat, Square, Hexagonal
Specifications
GBn 198-88, ГОСТ 10994-1974, ГОСТ 10160-1975, ASTM A753-2008
Common Name: Ni50, E11a, 50H, Hy-Ra49, PB
Cores of various transformers,
relays,
electromagnetic clutches and reactors in medium magnetic field,
pole shoes,
relay components of earth leakage breakers,
gas safety valves,
magnetic shielding,
gyroscopes,
automatic synchronous motors and mini size motors etcs.
Alloy | C | P | S | Si | Mn | Ni | Cu | Co | Cr | Fe |
---|---|---|---|---|---|---|---|---|---|---|
1J46 | ≤0.03 | ≤0.02 | ≤0.02 | 0.15-0.30 | 0.60-1.10 | 45.0-46.5 | ≤0.20 | – | – | Rest |
1J50 | ≤0.03 | ≤0.02 | ≤0.02 | 0.15-0.30 | 0.30-0.60 | 49.0-50.5 | ≤0.20 | – | – | Rest |
1J54 | ≤0.03 | ≤0.02 | ≤0.02 | 1.10-1.40 | 0.60-1.10 | 49.5-51.0 | ≤0.20 | – | 3.80-4.20 | Rest |
Alloy | Type | Class | Thickness, mm | Elastic permeability at different frequencies measured at the peak value of magnetic field intensity of 0.4 A/m, μ1/mH˙m-1 | |||
---|---|---|---|---|---|---|---|
60 Hz | 400 Hz | 1 kHz | 10 kHz | ||||
1J50 | Cold rolled strip | Ⅱ | 0.02 | – | – | ≥2000(2.5) | ≥1600(2.0) |
0.05 | – | – | ≥2000(2.5) | ≥1440(1.8) | |||
0.10 | – | ≥3120(3.9) | ≥3040(3.8) | – | |||
0.20 | – | ≥3040(3.8) | ≥2400(3.0) | – | |||
0.35 | ≥4000(5.0) | ≥3040(3.8) | – | – |
Alloy | Type | Class | Thickness, mm | Permeability at a magnetic field intensity of 0.4 A/m, μ0.4/mH˙m-1 | Maximum permeability μm/mH˙m-1 | Coercive force (under saturation magnetic induction) Hc/A˙m-1 | Saturation magnetic induction Bs/T |
---|---|---|---|---|---|---|---|
1J46 | Cold rolled strip | 0.03-0.04 | ≥1280(1.6) | ≥18000(22.5) | ≤32 | 1.5 | |
0.05-0.09 | ≥1600(2.0) | ≥22000(27.5) | ≤24 | 1.5 | |||
0.10-0.19 | ≥2000(2.5) | ≥25040(31.3) | ≤20 | 1.5 | |||
0.20-0.34 | ≥2480(3.1) | ≥30000(37.5) | ≤16 | 1.5 | |||
0.35-2.50 | ≥2800(3.5) | ≥36000(45.0) | ≤12 | 1.5 | |||
Hot rolled flat | 4.5-20 | ≥2000(2.5) | ≥25040(31.3) | ≤16 | 1.5 | ||
Hot rolled rod | 20-100 | ≥2000(2.5) | ≥25040(31.3) | ≤16 | 1.5 | ||
1J50 | Cold rolled strip | Ⅰ | 0.05-0.09 | ≥2000(2.5) | ≥28000(35) | ≤20 | 1.5 |
0.10-0.19 | ≥2320(2.9) | ≥32000(40) | ≤14.4 | 1.5 | |||
0.20-0.34 | ≥2640(3.3) | ≥40000(50) | ≤11.2 | 1.5 | |||
0.35-0.50 | ≥3040(3.8) | ≥50000(62.5) | ≤9.6 | 1.5 | |||
0.51-1.00 | ≥3040(3.8) | ≥50000(62.5) | ≤9.6 | 1.5 | |||
1.10-2.50 | ≥2800(3.5) | ≥45040(56.3) | ≤9.6 | 1.5 | |||
Ⅱ | 0.10-0.19 | ≥3040(3.8) | ≥35040(43.8) | ≤12 | 1.5 | ||
0.20-0.34 | ≥3520(4.4) | ≥45050(56.3) | ≤10.4 | 1.5 | |||
0.35-0.50 | ≥4000(5.0) | ≥52000(65) | ≤8.8 | 1.5 | |||
0.51-1.00 | ≥4000(5.0) | ≥40000(50) | ≤10 | 1.5 | |||
1.10-2.50 | ≥3040(3.8) | ≥35200(44) | ≤12 | 1.5 | |||
Ⅲ | 0.05-0.20 | ≥10000(12.5) | ≥60000(75) | ≤4.8 | 1.52 | ||
Hot rolled flat | 4.5-20 | ≥2480(3.1) | ≥25040(31.3) | ≤14.4 | 1.5 | ||
Hot rolled rod | 20-100 | ≥2480(3.1) | ≥25040(31.3) | ≤14.4 | 1.5 | ||
1J54 | Cold rolled strip | Ⅰ | 0.03-0.04 | ≥1520(1.9) | ≥16000(20) | ≤20 | 1.0 |
0.05-0.09 | ≥2000(2.5) | ≥20000(25) | ≤16 | 1.0 | |||
0.10-0.19 | ≥2480(3.1) | ≥25040(31.3) | ≤12 | 1.0 | |||
0.20-0.34 | ≥3040(3.8) | ≥28000(35) | ≤9.6 | 1.0 | |||
0.35-0.50 | ≥3200(4.0) | ≥32000(40) | ≤8 | 1.0 | |||
0.51-1.00 | ≥3040(3.8) | ≥32000(40) | ≤8 | 1.0 | |||
Ⅱ | 0.03-0.04 | ≥3040(3.8) | ≥24800(31) | ≤12 | 1.0 | ||
0.05-0.09 | ≥3040(3.8) | ≥24800(31) | ≤12 | 1.0 | |||
0.10-0.19 | ≥3120(3.9) | ≥28000(35) | ≤10 | 1.0 | |||
0.20-0.34 | ≥3120(3.9) | ≥30000(37.5) | ≤10 | 1.0 | |||
0.35-0.50 | ≥3520(4.4) | ≥35200(44) | ≤8 | 1.0 |
Note: Saturation magnetic induction Bs is measured at a magnetic field intensity between 2000A/m and 24000A/m.
Q: Would you provide samples For free?
A: Yes . with on stock specification We provide samples For Free . Freight charge collect
![]() |
1J50 E11a 0.2 Mm Stainless Steel Plates Soft Magnetic Sheet Hyra 49 Images |